摘要(Abstract):

针对出砂井因上覆地层沉降与射孔段地层空洞而导致的射孔套管变形问题,采用有限元分析软件,建立考虑上覆地层位移与出砂空洞的射孔套管变形分析模型,采用经典Lame公式验证模型的正确性,分析射孔孔眼密度、孔径和射孔相位角对射孔套管变形的影响。结果表明:出砂井射孔套管在轴向载荷作用下的变形不同于在径向挤压作用下的变形,微小的上覆地层位移就能导致射孔套管发生大变形;当射孔孔眼密度为25~30 m~(-1),孔径为13~15 mm,相位角为45°、60°或90°时,能够有效减小上覆地层位移造成的射孔套管变形。

关键词(KeyWords): 出砂井;射孔套管;射孔参数;变形分析模型;上覆地层位移

基金项目(Foundation): 国家重点研发计划项目(2018YFC0310201);; 中国博士后科学基金特别资助(站前)项目(2021TQ0273)

作者(Author): 姜广彬,郭晓强,张瑞霞,柳军

DOI: 10.13349/j.cnki.jdxbn.20210901.005

参考文献(References):

[1] YU H,LIAN Z H,LIN T J,et al.Experimental and numerical study on casing wear in highly deviated drilling for oil and gas[J].Advances in Mechanical Engineering,2016,8(7):1-15.

[2] 党兴武.基于35CrMo/GCr15摩擦副的疲劳磨损机理研究[D].兰州:兰州理工大学,2017.

[3] MATSUMOTO K,SAGARA M,MIYAJIMA M,et al.Study of oil country tubular goods casing and liner wear mechanism on corrosion-resistant alloys[J].SPE Drilling & Completion,2018,33(1):41-49.

[4] PARK C Y,RHEE H,RYU K W.Wear depth prediction for steam generator tubes using an estimated in situ wear coefficient[J].Nuclear Technology,2018,201(1):23-40.

[5] YU H,TALEGHANI A D,LIAN Z H.Modelling casing wear at doglegs by incorporating alternate accumulative wear[J].Journal of Petroleum Science and Engineering,2018,168:273-282.

[6] GUO J,FAN S,LIU T,et al.Exploration and practice of integrated control technology for tubing and sucker rod lopsided wearing in directional well[C]//2018 International Conference on Air Pollution and Environmental Engineering (APEE 2018),October 26-28,2018,Hong Kong,China:Vol 208.Bristol:IOP Publishing,2018:012021.

[7] 徐学利,王涛,余晗,等.低摩擦速度下CT80油管摩擦磨损性能[J].润滑与密封,2019,44(2):66-71.

[8] GUO X Q,LIU J,DAI L M,et al.Friction-wear failure mechanism of tubing strings used in high-pressure,high-temperature and high-yield gas wells[J].Wear,2021,468/469(2):203576.

[9] MAO L J,CAI M J,TIAN J,et al.Effect of drilling fluid type on wear behavior of casing[J].Journal of Materials Science and Engineering,2020,38(3):482-487.

[10] MAO L J,CAI M J,WANG G R.Effect of rotation speed on the abrasive-erosive-corrosive wear of steel pipes against steel casings used in drilling for petroleum[J].Wear,2018,410/411:1-10.

[11] 温诗铸,黄平,田煜,等.摩擦学原理[M].5版.北京:清华大学出版社,2018.

[12] 王志信,蔡景瑞.射孔对套管的损害及改进措施[J].测井技术,1984(5):33-37.

[13] 唐波,杨龙,练章华,等.射孔套管应力集中系数有限元分析[J].西南石油学院学报,2003,25(4):69-72.

[14] AI C,ZHAO W C,GUO B Y.Casing collapse strenth reduction under lateral loads from yielding shales in the Daqing Oilfield[J].SPE Drilling & Completion,2008,23(4):348-352.

[15] 张建忠,靳鹏菠,刘锋,等.出砂套管受力有限元分析[J].新疆石油天然气,2011,7(1):66-67,75.

[16] 张立民.冀东油田出砂井射孔套管变形分析[J].石油钻采工艺,2013,35(5):71-73.

[17] GUO Y G,BLANFORD M,CANDELLA J.Evaluating the risk of casing failure caused by high-density perforation:a 3D finite-element-method study of compaction-induced casing deformation in a deepwater reservoir,Gulf of Mexico[J].SPE Drilling & Completion,2015,30(2):141-151.

[18] SCHEPERBOER I,EFTHYMIOU E,MALJAARS J.Deformation of perforated aluminium plates under in-plane compressive loading[J].Key Engineering Materials,2016,710:357-362.

[19] 姬丙寅,曹传文,刘彦,等.套管射孔后抗挤强度有限元分析[J].钢管,2018,47(2):72-75.

[20] 李明飞,窦益华,曹银萍,等.考虑套管边界和液柱高压的射孔液压力脉动规律分析[J].振动与冲击,2019,38(24):189-196.

[21] 逄铭玉,许高,唐英才,等.井下环境固井水泥环射孔冲击破坏实验研究[J].测井技术,2019,43(4):348-354.

[22] 孙宝江,彭玉丹,张伟国,等.筛管压溃强度计算公式及适用性[J].石油学报,2020,41(3):363-371.

[23] 许杰,贾立新,陈毅,等.海上稠油热采井套管射孔参数设计[J].中国海上油气,2020,32(3):118-123.

[24] 李明飞,窦益华,曹银萍,等.射流速度及套管应力的ALE三维仿真分析[J].力学季刊,2019,40(2):362-372.

[25] 黎伟,陈曦,夏杨,等.机加工孔套管抗挤压强度有限元分析[J].过程工程学报,2020,20(2):189-196.

[26] 曹银萍,李明飞,窦益华,等.爆轰与聚能射流下射孔枪和套管的应力强度耦合仿真分析[J].石油钻采工艺,2019,41(4):480-488.

[27] 李明飞,窦益华,刘玉雪.射孔套管应力强度及影响因素仿真分析[J].计算机仿真,2020,37(3):100-105,133.

[28] 陈华彬,唐凯,李妍僖,等.爆炸耦合载荷作用的射孔套管强度模拟分析[J].石油矿场机械,2020,49(3):15-23.

[29] TIMOSHENKO S P,GOODIER J N.Theory of Elasticity[M].3rd ed.London:McGrawHill Book Company,1970.

[30] 张皓斌.厚壁圆筒强度及开孔补强的分析与讨论[J].化工设计,2020,30(6):19-24.